Introduction:
DSC is designed to determine the inner heat transition relating to temperature and heat flow, it is widely
used in the field of polymer development, performance testing & quality control. DSC research and
development includes the following field: glass transition temperature, melting point, cold crystallization,
crystallization, phase transition, oxidation induction time (OIT).
Standards:
ISO/TR10837:1991, ASTM D3895-1998, ASTM E 967, ASTM E 968, ASTM E 793, ASTM D 3895,
ASTM D 3417, ASTM D 3418, ISO 11357-6
Main Features:
1. New designed oven structure ensures high resolution and good stability of base line;
2. Air flow meter may control the air flow rate accurately; the test data can be recorded

3. The instrument is bilateral control, may be controlled by both main frame and software.

Technical parameters:
1. DSC range: 0
±500mW
2. Temperature range: room temperature ~ 800
air-cooled
3. Heating rate: 1 ~ 80
/ min
4. Cooling rate * : 1 ~ 20
/ min (OPTIONAL)
5. Temperature resolution: 0.1

6. Temperature fluctuations: ±0.1

7. Temperature repeatability: ±0.1

8. DSC noise: 0.01μW
9. DSC resolution: 0.01μW
10. DSC accuracy: 0.1 u W
11. DSC sensitivity: 0.1 u W
12. Control Mode: Rising temperature, constant temperature(full automatic programmed control)
13. Curve scanning: Rising scan, *cooling scan (OPTIONAL)
14. Gas flow control: Embedded digital flow meter & Software control, automatic changing
15. Color: 24 bit 7 inches LCD touch screen display

16. Data interface: standard USB connector

17. Parameter standard: equipped with standard material, with a key calibration function, the user may
correct temperature and heat enthalpy
Packing list: 

 

Host instrument 

1

CD 

1

Data Line     

1

Power Line        

1

Aluminum crucibles

400

Ceramic crucibles    

100

Bag of pure tin grains

1

Fuse 4A    

5

Operation manual 

1

Warranty card  

1

Certification     

1

 

Name
*
Mobile
*
Email
*
Content
*