			1: Temperature sensitivity up to 0.001
2: The software has multi analysis functions, which can open multiple curves for analysis
3: Metal U-shaped furnace body, good repeatability
4.Can measure multi test items, includes OIT, Tg and melt point
5.TUV &CE certification 
DSC is designed to determine the inner heat transition relating to temperature and heat flow, it is widely used in the field of polymer development, performance testing & quality control. DSC research and development includes the following field: glass transition
temperature, melting point, cold crystallization, crystallization, phase transition, oxidation induction time (OIT).
Standards:
ISO/TR10837:1991, ASTM D3895-1998, ASTM E 967, ASTM E 968, ASTM E 793, ASTM D 3895, ASTM D 3417, ASTM D 3418, ISO 11357-6
Main Features:
1. New designed oven structure ensures high resolution and good stability of base line
2. Air flow meter may control the air flow rate accurately; the test data can be recorded
3. It is bilateral control, may be controlled by both main frame and software.
Parameters:
| Temperature range | -40℃ ~ 600 ℃ | 
| Heating rate | 0.1~100℃/min | 
| Temperature resolution | 0.01 ℃ | 
| Temperature fluctuations | ±0.01℃ | 
| Temperature repeatability | ±0.1℃ | 
| Constant temperature time | Program setting ≤24h | 
| DSC range | 0~±600mW | 
| DSC noise | 0.01μW | 
| DSC resolution | 0.01μW | 
| DSC accuracy | 0.01mW | 
| Atmosphere control gas | Nitrogen, Oxygen (instrument switch automatically) | 
| Gas flow rate | 0-300mL/min | 
| Gas pressure | 0.2MPa | 
| Control Mode | Rising temperature, cooling ,constant temperature(full automatic) | 
| Curve scanning | Rising scan, cooling scan | 
| Gas flow control | Built-in digital flow meter & Software control, automatic | 
| Display | 24 bit 7 inches LCD touch screen display | 
| Data interface | standard USB connector | 
| Parameter standard | With standard material, with calibration function, the | 
| user may correct temperature and heat enthalpy | |
| Software | Professional control operating software | 
| Thermocouples | Total 3 sets of thermocouples for: 1). Test sample temperature 2). test furnace temperature, 3). Test internal ambient temperature | 
| Cooling device | Semiconductor refrigeration | 
| Power | AC220V/50Hz | 
Packing List
| Host instrument | 1 | 
| CD | 1 | 
| Data Line | 1 | 
| Power Line | 1 | 
| Aluminum crucibles | 100 | 
| Ceramic crucibles | 100 | 
| pure tin grains | 1bag | 
| Fuse 4A | 5 | 