[language-switcher]
SKZ1052C-1L Differential Scanning Calorimeter
5
6
4

SKZ1052C-1L Differential Scanning Calorimeter

1. Temperature sensitivity up to 0.001.
2. The software has multi – analysis functions, allowing for the simultaneous analysis of multiple curves.
3. Metal U – shaped furnace body provides excellent repeatability.
4. Can measure various items like OIT, Tg, and melting point.
5. Holds TUV & CE certifications, meeting international standards.

Get a quote

Products details:

DSC is designed to determine the inner heat transition relating to temperature and heat flow, it is widely used in the field of polymer development, performance testing & quality control. DSC research and development includes the following field: glass transition temperature, melting point, cold crystallization, crystallization, phase transition, oxidation induction time (OIT).

Standards:
ISO/TR10837:1991, ASTM D3895-1998, ASTM E 967, ASTM E 968, ASTM E 793, ASTM D 3895, ASTM D 3417, ASTM D 3418, ISO 11357-6

Main Features:
1. The industrial-grade 7-inch touch screen displays rich information.
2.Brand-new metal furnace body structure, with better baseline and higher accuracy.
The heating adopts indirect conduction method, which has high uniformity and stability, reduces pulse radiation, and is better than traditional heating mode.
3. USB communication interface, strong versatility, reliable and uninterrupted communication, supports self-recovery connection function.
4. Automatically switch the two-channel atmosphere flow, fast switching speed and short stabilization time. At the same time, a protective gas input is added.
5. The software is simple and easy to operate.

Technical parameters:

Temperature range -150℃~ 600 ℃   
Heating rate 0.1~80℃/min
Cooling rate 1 ~ 20 ℃ / min  (If cooling, For instant cool only, can not be Isothermal below room temperature, and if heating up, can control its rate)
Temperature resolution 0.001℃
Temperature fluctuations ±0.001℃
Temperature repeatability ±0.1℃
Constant temperature time Program setting ≤24h
DSC range 0~±600mW
DSC noise 0.01μW
DSC resolution 0.01μW
DSC accuracy 0.01mW
Atmosphere control gas Nitrogen, Oxygen (instrument switch automatically)
Gas flow rate 0-300mL/min
Gas pressure 0.2MPa
Control Mode Rising temperature, constant temperature(full automatic)
Curve scanning Rising scan, cooling scan 
Gas flow control Built-in digital flow meter & Software control, automatic
Display 24 bit 7 inches LCD touch screen display
Data interface standard USB connector
Parameter standard With standard material, with calibration function, the user may correct temperature and heat enthalpy
Software operating software
Thermocouples  Total 3 sets of thermocouples for:

1). Test sample temperature

2). test furnace temperature,

3). Test internal ambient temperature

Cooling device Liquid nitrogen refrigeration
Power AC220V/50Hz
Pressure gauges Gas flow meter
Whether it requires a specific surface No, horizontal surface is ok
Note All technical indicators can be adjusted according to the user needs

Packing List

Host instrument 1PC
CD 1PC
Data Line 1PC
Power Line 1PC
Aluminum crucibles 100PCS
Ceramic crucibles 100PCS
pure tin grains 1bag
Fuse 4A 5PCS